Attention: During the process of EPS beads pre-expanding in Pre-Expander !
EPS production technology: Pre-expansion
-
Excessive steam residence time and superheated steam will cause damage to EPS beads
-
Prevent steam from overheating: Do not use thermal insulation material to keep the last 5-8 meters steam pipe from the steam pressure reducing valve to the pre-expander
-
Pressure: 0.2-1.2bar = low heat content
-
Must contain some moisture to create a condensation layer on the EPS surface to slow the transfer of heat to the EPS particles.
-
Pre-expand EPS particles smoothly & uniformly